Case 1: White bronze deposit is not wear-resistant, how to solve it? Case 2: How to solve the problem that deposition nickel-free gold is not corrosion-resistant? Case 3: How to make gold deposition become more wear-resistant? Case 4: What is the best plating process for 925 Jewelry? Case 5: Example for 12K light thick gold(3µm) Case 6: Example for environment-friendly thick white bronze
Case 1: Example for settling the claim for compensation for Non-environment-friendly element thallium Case 2: Electro-coating over white bronze,No change in color Case 3: Example for wear-resistant hard silver Case 4: Example for wear-resistant hard gold plating
Case 1: Ternary alloy(Copper-Tin-Zinc)dry under 260℃ for 40 minutes,No change in color Case 2: Example for ternary alloy(Copper-Tin-Zinc) how to pass 720h Neutral Salt Spray test
Case 1: Imitation gold how to replace 24K real gold
Case 1: Bright yellow bronze replace acid copper plating Case 2: 24K gold imitation with electro-coating, how to keep fresh color Case 3: Example for barrel plating of gold imitation (24K) Case 4: Example for barrel plating of coffee gold imitation Case 5: Example for raser and sand sweeping of thick white bronze
Case 1:Example for nickel-free environment-friendly plating for sanitary products